Seal Strength Testing: Methods, Equipment and Packaging Standards

Tensile testing machine performing seal strength test on packaging with force displacement graph

@import url(‘https://fonts.googleapis.com/css2?family=Inter:wght@400;500;600;700;800&display=swap’);
.vc-article{font-family:’Inter’,sans-serif;color:#1a1a2e;line-height:1.7;max-width:820px;margin:0 auto}
.vc-article p{font-size:17px;margin:0 0 18px 0}
.vc-article b,.vc-article strong{font-weight:700}
.vc-article a{color:#2563eb;text-decoration:none;font-weight:700}
.vc-article a:hover{text-decoration:underline}
.vc-article h2{font-size:26px;font-weight:800;margin:48px 0 20px 0;letter-spacing:-0.3px}
.vc-article h3{font-size:20px;font-weight:700;margin:32px 0 12px 0}
.vc-stat-line{background:#f3f4f6;padding:16px 20px;margin:24px 0;font-size:17px;line-height:1.6}
.vc-stat-line b{font-size:20px;font-weight:800}
.vc-table-wrap{margin:24px 0}
.vc-table-wrap table{width:100%;border-collapse:collapse;border:1px solid #e5e5e5}
.vc-table-wrap th{padding:12px 16px;text-align:left;background:#1a1a2e;color:#fff;font-size:14px;font-weight:600;text-transform:uppercase;letter-spacing:0.3px}
.vc-table-wrap td{padding:12px 16px;border-bottom:1px solid #e5e5e5;font-size:15px}
.vc-table-wrap tbody tr:nth-child(even){background:#f9f9fb}
.vc-callout{background:#fef3c7;padding:16px 20px;margin:24px 0;font-size:16px;line-height:1.6}
.vc-callout b{color:#92400e}
.vc-steps{margin:24px 0}
.vc-step{display:flex;gap:16px;padding:18px 20px;background:#f8f8fa;margin-bottom:2px;align-items:flex-start}
.vc-step:nth-child(even){background:#fff;border:1px solid #eee}
.vc-step-num{background:#1a1a2e;color:#fff;width:34px;height:34px;display:flex;align-items:center;justify-content:center;font-size:15px;font-weight:800;flex-shrink:0}
.vc-step-content{flex:1}
.vc-step-title{font-weight:700;font-size:16px;margin-bottom:4px}
.vc-step-desc{font-size:15px;color:#444;line-height:1.6}
@media(max-width:600px){
.vc-article p{font-size:16px}
.vc-article h2{font-size:22px;margin-top:36px}
.vc-article h3{font-size:18px}
.vc-stat-line b{font-size:18px}
.vc-step{padding:14px 16px}
.vc-table-wrap table,.vc-table-wrap thead,.vc-table-wrap tbody,.vc-table-wrap th,.vc-table-wrap td,.vc-table-wrap tr{display:block}
.vc-table-wrap thead{position:absolute;top:-9999px;left:-9999px}
.vc-table-wrap tr{margin-bottom:16px;border:1px solid #e5e5e5;background:#fff !important}
.vc-table-wrap td{padding:10px 14px;border:none;border-bottom:1px solid #f0f0f0;position:relative;padding-left:40%}
.vc-table-wrap td:last-child{border-bottom:none}
.vc-table-wrap td::before{content:attr(data-label);position:absolute;left:14px;top:10px;font-weight:700;font-size:12px;color:#1a1a2e;text-transform:uppercase;letter-spacing:0.3px;width:35%;white-space:normal}
}

By Alex Hales

A weak seal does not usually fail on the production line. It fails three days later in the back of a delivery truck, or on a shelf under a heat lamp, and by then the recall is already expensive. Seal strength testing is how packaging teams catch that failure before a customer does, by measuring the exact force it takes to pull a seal apart.

The industry runs on one number more than any other. ASTM F88 is the standard nearly every peel test traces back to, and it is the test most auditors ask to see first when they walk into a packaging QA lab.

Most flexible packaging lines run peel tests at 8 to 12 inches per minute using a tensile tester, pulling a 1-inch strip until the seal separates or the material tears.

Seal strength and seal integrity get used interchangeably a lot, and that mix-up causes real problems downstream. Seal strength tells you how much force a seal can take before it comes apart. Seal integrity tells you whether the package is actually sealed shut with no pinholes or channels for contamination to sneak through.

A seal can pass a strength test and still leak. It can also look solid under a microscope and still peel apart at half the force your spec calls for. Running both types of test, not just one, is the difference between a packaging line that passes audits and one that gets flagged.

This guide walks through the methods, the equipment, and the standards a QA manager or packaging engineer actually needs to build a testing protocol that holds up. That starts with getting clear on what seal strength testing covers and where it stops.

What Seal Strength Testing Actually Covers

Seal strength testing applies almost everywhere a package gets heat sealed. That includes flexible pouches, sachets and stick packs, medical device packaging, food packaging, and pharmaceutical blister and pouch packaging. Anywhere a bag or lidding film gets bonded shut, someone downstream needs to know how strong that bond is.

The core idea is simple even though the testing gets technical fast. You apply a measured, controlled force to a sealed sample until it separates, and you record how much force that took. Do that enough times across a production run and you get a real picture of whether your sealing process is consistent or drifting.

What seal strength testing will not tell you is whether the package leaks. A seal can hit its target peel force and still have a microscopic channel running through it, especially on curved or textured film. That is a job for a separate category of tests, which we will get to further down.

Knowing the difference matters because a lot of QA programs test for one and assume they have covered both. The next question is which strength test fits your packaging, and the answer usually starts with peel testing.

Peel Testing: The Workhorse Method (ASTM F88)

Peel testing under ASTM F88 is the most common seal strength test in the industry, and it is probably the one your customers or auditors will ask about by name. A 1-inch wide strip is cut from the sealed area and clamped into a universal tensile tester, which then pulls the two layers apart at a fixed angle, either 90 degrees or 180 degrees, at a steady speed.

The machine records force continuously through the pull, not just at the moment of failure. That gives you both an average peel force and a peak force, which matters because a seal that fails gradually behaves very differently from one that pops open all at once.

Peel testing is good at two things beyond a pass or fail number. It shows whether your seal strength is consistent across a roll of film, and it flags weak spots before they become customer complaints. A seal that peels evenly at 4 lbf across ten samples tells a very different story than one that ranges from 2 to 6 lbf on the same batch.

Peel testing tells you how strong a seal is at rest, but it says nothing about what happens the instant that seal comes off the sealing jaws. That gap is exactly what hot tack testing was built to close.

Hot Tack Testing: Catching Failures in the First Second

On a vertical form fill seal (VFFS) machine, product drops into the bag within a second or two of the seal being formed, while the film is still hot and the bond has not fully set. If the seal cannot hold weight at that exact moment, the bag opens on the line and nobody finds out until product is on the floor.

Hot tack testing under ASTM F1921 measures seal strength immediately after sealing, while the material is still warm, rather than after it has cooled to room temperature like a standard peel test. This is the test that catches problems peel testing misses entirely, because a seal can have excellent cold peel strength and still fail hot tack if the sealant layer is slow to set.

Hot tack data matters most for high-speed fill lines running liquids, powders, or granular product where the fill happens fast and the seal has no time to rest. If your line runs VFFS equipment, this test is not optional, it is the one that predicts what actually happens on your floor.

Hot tack and peel testing both measure a seal pulling apart under a steady, controlled load. Burst testing takes a completely different approach, pressurizing the whole package until something gives.

Burst Testing: Finding the Weakest Point

Burst testing, covered under ASTM F1140 and ASTM F2054, fills a sealed package with air like a balloon and keeps increasing internal pressure until the weakest part of the package fails, whether that is a seal or the film itself. Unlike peel testing, which isolates one strip of seal, burst testing evaluates the whole package as a system.

This is the method to reach for on liquid pouches, vacuum packaging, and any flexible package where internal pressure changes during shipping or storage, such as products that ship by air. A burst tester applies regulated, steadily increasing air pressure and records the exact pressure at the moment of failure, along with where on the package that failure happened.

Burst testing is also the fastest way to spot a design flaw that peel testing would never catch, like a corner seal that is fine in isolation but becomes the weak point once the whole package is under load. Corners, fitments, and seal intersections fail more often in burst tests than flat seal areas do.

Peel, hot tack, and burst testing all answer the same underlying question from different angles: how much force can this seal take right now. Creep testing asks a different question entirely, which is how that seal holds up over time.

Creep Testing: Simulating Weeks on a Shelf or Truck

A creep test applies a constant, sustained pressure to a sealed package and then just watches it, sometimes for hours, sometimes for days, monitoring for slow leaks or gradual seal failure. This is not about finding a breaking point the way burst testing is. It is about finding out whether a seal that looks fine today will still be fine after a week in a hot warehouse or a long haul in an unpressurized truck.

Creep testing is where shelf-life claims actually get proven. A package that passes peel and burst tests on day one can still fail creep testing if the seal relaxes under sustained low-level stress, which is a common issue with certain laminate structures and adhesive-based seals.

Running creep tests is slower and less common than the other three methods, which is exactly why skipping it is risky. It is usually the method that catches problems the faster tests miss.

Method Standard What It Measures Best Fit
Peel testing ASTM F88 Force to separate a seal at rest General flexible packaging, seal consistency checks
Burst testing ASTM F1140 / F2054 Maximum internal pressure before failure Liquid pouches, vacuum packaging
Hot tack testing ASTM F1921 Seal strength immediately after sealing VFFS lines, fast-fill applications
Creep testing No single ASTM standard Seal durability under sustained pressure over time Shelf-life validation, long-haul shipping

Four different tests, four different failure modes. But strength is only half the picture, because a seal can hold together under every one of these tests and still let contamination through a gap nobody can see.

Seal Integrity Testing: The Other Half of the Picture

Seal integrity tests do not measure force at all. They are built to find leaks, channels, and pinholes that a strength test would never catch, since a seal can peel apart at full spec strength and still have a defect running through it.

The bubble leak test under ASTM F2096 submerges a pressurized package in water and watches for escaping air bubbles, which is a cheap and fast way to spot a leak visually. Dye penetration testing under ASTM F1929 pushes a colored liquid through the seal area, and any hidden channel or gap shows up as a visible stain. Both are manual, low-cost, and good for spot checks on a production line.

Vacuum decay testing and pressure decay testing are the more sensitive, instrument-based versions of the same idea. The package sits in a chamber and the equipment monitors pressure changes over time, catching leaks far smaller than a visual bubble test ever could, without damaging the sample. For liquid-filled packages, high voltage leak detection uses electrical conductivity to find microscopic defects that none of the pressure-based methods can see.

Integrity Method Standard How It Works
Bubble leak test ASTM F2096 Submerge pressurized package, watch for bubbles
Dye penetration ASTM F1929 Colored liquid reveals channel leaks
Vacuum decay No single ASTM standard Chamber monitors pressure change for micro-leaks
Pressure decay No single ASTM standard Measures pressure loss over time inside the package
High voltage leak detection No single ASTM standard Electrical conductivity finds microscopic defects

Strength testing and integrity testing solve different problems, and a mature QA program runs both. Once you know which tests you need, the next decision is what equipment actually runs them.

The Equipment Behind Every Result

Universal tensile testers are the backbone of any seal strength lab, pulling samples apart at steady speeds, typically 8 to 12 inches per minute, using pneumatic grips that hold film without slipping or tearing at the clamp point. This is the machine running your ASTM F88 peel tests day to day, and it is worth buying one built for film rather than a general-purpose model, since flexible packaging behaves very differently under a pneumatic grip than rigid materials do.

Burst testers apply regulated, controlled internal air pressure to a sealed package and record the exact pressure and location of failure. Hot tack testers combine a heat sealer and a tensile tester into one unit, sealing a sample and pulling it apart within a set, repeatable time window measured in fractions of a second.

None of these tests mean anything if your test samples were not made correctly in the first place, which is where laboratory heat sealers come in. A good lab sealer controls temperature, dwell time, and pressure precisely enough that every sample going into a tensile tester was sealed under identical conditions, matching the process detailed in ASTM F2029 for specimen preparation. Vanguard Components supplies tensile testers, burst testers, and lab heat sealers built around exactly this kind of repeatability, since inconsistent sample prep is one of the most common reasons two labs get different numbers off the same roll of film.

Good equipment removes variables from the test itself. It cannot fix a sealing process that was already inconsistent on the production line, which brings up the factors that actually determine whether a seal is strong in the first place.

Five Variables That Quietly Wreck Seal Strength

Sealing temperature is the most common culprit behind inconsistent seals. Run it too low and the layers never bond properly. Run it too high and you burn or deform the material, which can look fine visually while the seal underneath is already compromised.

Dwell time, meaning how long the sealing jaws stay in contact with the film, works the same way. Too short and the seal never fully forms. Too long and you risk damaging the material even at a correct temperature, which is why dwell time and temperature always get tuned together rather than in isolation.

Sealing pressure needs to be even across the entire seal area. Uneven pressure creates weak spots and channel leaks even when the average pressure reading looks correct, because a slightly misaligned jaw can produce a seal that passes a spot check and fails in the field.

Packaging material itself plays a bigger role than most people expect. Thickness, sealant layer composition, and overall laminate structure all change how a material responds to the exact same heat, pressure, and dwell settings, which is why switching suppliers on the same film spec can still shift your peel numbers.

Machine condition rounds out the list, and it is the one that gets ignored longest because it degrades slowly. Worn sealing jaws, a damaged heating element, or a machine that has drifted out of alignment will produce weaker seals long before anyone notices on a visual inspection, which is exactly why routine strength testing matters even on lines that have run the same product for years.

Matching Standards to Your Packaging Type

Not every ASTM standard applies to every product, and picking the wrong one wastes lab time without telling you anything useful. ASTM F88 is the default for general flexible barrier materials. ASTM F2824 exists specifically for peelable lids on round containers, which F88’s flat-strip method was never designed to handle well.

ASTM F1140 and F2054 cover burst testing for non-restrained packages, while ASTM F1921 is the one to reach for on any VFFS or fast-fill line. Medical device and pharmaceutical packaging usually needs to satisfy ISO 11607, the global standard for sterile barrier packaging validation, which pulls together strength testing, integrity testing, and shelf-life data into one validation package rather than treating them as separate exercises.

Getting the standard right up front saves rework later, especially for regulated products where an auditor will ask which standard a test method traces back to. That question of fit, matching the right test to the right packaging, is really the whole point of building a testing protocol instead of just running whatever test is fastest.

A seal strength protocol built on the right combination of peel, burst, hot tack, and integrity testing catches problems long before they reach a customer or an auditor. If your lab needs a tensile tester, burst tester, or lab heat sealer built for exactly this kind of testing, get in touch with Vanguard Components for a spec sheet and a quote.

Frequently Asked Questions

Latest Blogs

Pneumatic cylinder with a blank label beside digital calipers and an O-ring on a white lab bench

Replacement Part With No Part Number? How to Find the Match

White packaging conveyor belt with stainless steel side guides carrying cartons

Packaging Conveyor Belt Problems: Mistracking, Slipping and Fraying Fixed in Order

Vertical form fill seal machine with forming tube, sealing jaws and a filled clear bag

VFFS Seal Problems: Leaks, Wrinkles and Burn-Through, and What to Fix First

Contact Us

or

Get a quote

Get a quote